A.Blended Polyol

ItemIndex
Material Temperature20~25℃
Mold Temperature45~60℃
Cream Time6~10s
Rising Time40~80s
Demold Time120~240s
POL/ ISO Ratio100:40~65

*The actual reactivity characteristics may be adjusted according to process conditions and clients’ requirements


B.ISO

BrandNCO%Details
JHW859825.8Modified MDI, widely operation window
JHW852928.5Modified MDI, widely operation window
JHW853226.5Modified MDI, widely operation window
JHW880335.3Mixed Modified MDI,apply in PIP headrest, Good liquidity